Stress-Strain Curves

The stress-strain curve visualizes how a material behaves under load, showing the relationship between applied stress and resulting strain.


Regions of the Curve

1. Linear Elastic Region

  • Stress proportional to strain (Hooke's Law)
  • Strain is reversible
  • Slope = Young's Modulus (E)
  • Ends at proportional limit

2. Nonlinear Elastic Region

  • Slight deviation from linearity
  • Still reversible
  • Ends at yield point

3. Plastic Region

  • Permanent deformation occurs
  • Strain increases faster than stress
  • Ends at ultimate tensile strength

4. Necking

  • Localized reduction in cross-section
  • Stress drops on engineering curve
  • Ends at fracture

Key Points

Point Description
P Proportional limit — linear relationship ends
Y Yield point — plastic deformation begins
U Ultimate strength — maximum stress
F Fracture — material breaks

Engineering vs. True Stress

Engineering Stress

σE=FA0\sigma_E = \frac{F}{A_0}

Uses original cross-sectional area.

True Stress

σT=FA\sigma_T = \frac{F}{A}

Uses instantaneous area.

Relationship

σT=σE(1+ε)\sigma_T = \sigma_E(1 + \varepsilon)


Ductile vs. Brittle

Ductile Materials (e.g., Steel, Aluminum)

  • Significant plastic deformation
  • Well-defined yield point
  • Necking before fracture
  • 20% elongation

Brittle Materials (e.g., Cast iron, Ceramic)

  • Little to no plastic deformation
  • Fracture at yield
  • No necking
  • <5% elongation

Strain Hardening

After yielding, additional load causes the material to become stronger.

σ=Kεn\sigma = K \varepsilon^n

  • K = Strength coefficient
  • n = Strain hardening exponent
Material n
Aluminum 0.15
Copper 0.54
Steel 0.20

Effect of Temperature

  • Higher temperature → lower E, lower yield
  • At elevated temperatures, creep becomes significant