Fatigue & S-N Curves

Fatigue is progressive, localized structural damage under cyclic loading. Failure occurs at stresses below yield strength.


Fatigue Failure Process

  1. Crack initiation — at stress concentrations (notches, surface defects)
  2. Crack propagation — stable crack growth per cycle
  3. Sudden fracture — catastrophic failure when remaining area can't carry load

S-N Curves

Stress vs. Number of cycles to failure.

Terminology

  • S = Stress amplitude
  • N = Cycles to failure
  • S_f = Fatigue strength at N cycles

Key Fatigue Parameters

Stress Ratio (R)

R=σminσmaxR = \frac{\sigma_{min}}{\sigma_{max}}

Stress Amplitude (σ_a)

σa=σmax−σmin2\sigma_a = \frac{\sigma_{max} - \sigma_{min}}{2}

Mean Stress (σ_m)

σm=σmax+σmin2\sigma_m = \frac{\sigma_{max} + \sigma_{min}}{2}


S-N Curve Regions

High-Cycle Fatigue (HCF)

  • N > 10⁴ cycles
  • Stress below yield
  • Elastic deformation

Low-Cycle Fatigue (LCF)

  • N < 10⁴ cycles
  • Plastic deformation per cycle
  • Strain-based analysis

Fatigue Limits

Fatigue Limit (S_e)

Stress below which material never fails (theoretical infinite life).

Material S_e (approx)
Steel 0.5 × σ_uts
Aluminum No true limit
Titanium 0.4 × σ_uts

Fatigue Strength (S_f)

Stress at a specific N (e.g., 10⁶ or 10⁷ cycles).


Modifications to S-N

Mean Stress Effects

Goodman Relation:

σa=Se(1−σmσuts)\sigma_a = S_e \left( 1 - \frac{\sigma_m}{\sigma_{uts}} \right)

** Gerber Relation:**

σa=Se(1−(σmσuts)2)\sigma_a = S_e \left( 1 - \left(\frac{\sigma_m}{\sigma_{uts}}\right)^2 \right)


Factors Affecting Fatigue Life

Factor Effect
Surface finish Rough surfaces reduce life
Size Larger parts reduce life
Temperature Elevated T reduces life
Corrosion Dramatically reduces life
Notches Stress concentration
Residual stress Compressive = beneficial

Fatigue Life Estimation

Basquin's Law

σa=σf′(2N)b\sigma_a = \sigma_f' (2N)^b

  • σ_f' = fatigue strength coefficient
  • b = fatigue strength exponent (-0.05 to -0.12)

Coffin-Manson (Low-Cycle)

Δε2=σf′E(2N)b+εf′(2N)c\frac{\Delta\varepsilon}{2} = \frac{\sigma_f'}{E}(2N)^b + \varepsilon_f'(2N)^c


Cumulative Damage

Miner's Rule:

∑niNi=1\sum \frac{n_i}{N_i} = 1

  • n_i = cycles at stress i
  • N_i = fatigue life at stress i